О возможностях новой технологии минеральных покрытий для повышения износостойкости металлической поверхности при создании деталей вакуумной техники
С. 78–82.
Skazochkin A. V., Bondarenko G., Kislov S. V. et al., Письма о материалах 2025 Vol. 15 No. 4 P. 277–283
The article presents the results of comparative studies of wear resistance of railway wheel samples with surface modification by ultrafine mineral powders and without modification. The tested samples are made of standard railway wheels made of CT2sp steel (ordinary quality carbon steel — an analogue of Q215 steel (China), A192 steel (USA), and RSt34–2 steel ...
Added: December 9, 2025
Roghani H., Borhani E., Jafarian H. R. et al., Wear 2023 Vol. 526-527 Article 204895
In this research, AA1050/AA2024 layered composites were created through six cycles of the ARB process. In this direction, the effect of using the reinforcing nanoparticles and the initial aging process on the mechanical properties and microstructure were researched. Two sheets of AA1050 and one sheet of AA2024 alternatively were used to create the composite. Also, ...
Added: February 18, 2025
Samoilova O., Shaburova N., Samodurova M. et al., Journal of Thermal Spray Technology 2023 Vol. 32 No. 5 P. 1220–1229
In this work, the morphology, microstructure, and phase composition of Al0.25CoCrFeNiSi0.6 high-entropy alloy coating (HEAC) deposited on stainless steel by detonation spraying (DS) are investigated. The Al0.25CoCrFeNiSi0.6 HEA ingot was first prepared by induction melting and then crushed and ground to ≤ 100 µm using a planetary ball milling apparatus. Detonation spraying was carried out on a computerized ...
Added: February 18, 2025
Naseri M., Ahmad Ostovari Moghaddam, Shaburova N. et al., Materials Today Communications 2024 Vol. 38 Article 108036
In the present work, Al0.25CoCrFeNiCu and Al0.45CoCrFeNiSi0.45 high entropy alloys (HEAs) were fabricated by induction melting and then subjected to severe cold rolling (SCR) to induce an ultrafine lamellar microstructure. By using electron back scattered diffraction (EBSD) analysis, the microstructural features of the SCR processed HEAs were determined to be deformation bands, severely pancaked grains, and a refined lamellar microstructure. The ...
Added: January 23, 2025
Skazochkin A. V., Bondarenko G.G., Zukowski P., Приборы и методы измерений 2020 Vol. 11 No. 3 P. 212–221
The aim of the article was to study the hardness of a metal surface modified with ultrafine particles of minerals by two different methods (instrumental indentation and Vickers hardness measurement) and a comparative analysis of the measurement results obtained by these methods.Standard Vickers hardness measurements at loads of 0.025, 0.1, and 0.5 kgf showed a ...
Added: September 23, 2020
Skazochkin A. V., Bondarenko G.G., Żukowski P., Devices and Methods of Measurements (Belarus) 2019 Vol. 10 No. 3 P. 263–270
A comparative study of the wear resistance, hardness and modulus of elasticity of ENAW-2024 aluminum alloy samples with and without a mineral coating was carried out. The wear resistance of the samples was studied by the method of multi-cycle friction, which makes it possible to measure the physicomechanical properties of thin modified material layers at ...
Added: September 12, 2019
Skazochkin A. V., Bondarenko G.G., Kislov S. V., Journal of Engineering Science and Technology Review 2018 Vol. 11 No. 6 P. 138–143
The work investigates some tribological parameters of the surfaces of friction pairs made of steel, with mineral layers. A comparative study of the friction coefficient of 18CrNiMo7-6 steel specimens with and without a mineral coating is
performed. The lowest friction coefficient value was achieved for samples with mineral coating, without HFC hard
surfacing before creating a mineral ...
Added: March 6, 2019
Kislov S. V., Kislov V. G., Balasch P. V. et al., IOP Conference Series: Materials Science and Engineering (MSE) 2016 Vol. 110 No. 012096 P. 1–5
The article describes the advantages of the new technology of mineral coating of metal products for the friction pair of mechanical systems. It presents the research results of the wear rate of the samples made of 12X13 steel (X12Cr13) with mineral layers, in the experiments with a piston ring sliding inside a cylinder liner with ...
Added: February 24, 2016
Kislov S. V., Kislov V. G., Skazochkin A. V. et al., Russian Metallurgy (Metally) 2015 No. 7 P. 558–564
The structural changes that occur in the surface and surface layers of steel 20Kh13 and titanium alloy PT3V (Russian designation) samples after each stage of hardening due to a formed mineral surface layer are studied by optical microscopy, transmission electron microscopy, and scanning electron microscopy. Electric spark alloying, pressing, and ultrasonic processing are used to ...
Added: October 22, 2015
Кислов С. В., Кислов В. Г., Балаш П. В. et al., Нефтегазовое дело 2015 № 4 С. 231–254
Новая технология создания минеральных покрытий на металлической поверхности была использована для создания износостойких слоев на резьбовых соединениях стальных насосно-компрессорных труб. Выполнены сравнительные исследования и определен ресурс работы резьбового соединения стальных насосно-компрессорных труб в исходном состоянии и после нанесеения минерального слоя. По результатам испытаний сделан вывод о том, что упрочняющее минеральное покрытие увеличивает износостойкость резьбового соединения ...
Added: September 11, 2015
Bondarenko G., Kislov S., Skazochkin A. et al., , in: Proceedings of 9th international conference "New electrical and electronic technologies and their industrial implementation".: lublin University of Technology, 2015. P. 99–99.
In the report the results of investigations of structural changes on a surface and in near-surface layers of samples from steel 20Cr13 (Rus.) and a titanic alloy of PT-3V (Rus) after each stage of creation of the strengthening mineral blanket on the offered technology have been presented. Use of an electrospark alloying, application of pressure ...
Added: July 15, 2015
Vasin V. A., Ivashov E., Кузнецов П. С. et al., Структурная Надёжность 2011 № 2 С. 40–48
Представлены методы расчёта трибоэкологических параметров, влияющих на загрязнение внутрикамерных объёмов вакуумного оборудования и дефектность, привносимую на обрабатываемые изделия электронной техники. Выполнен расчёт коэффициентов трения материалов, работающих в вакууме в зависимости от разряжения окружающей среды для случаев упругого и пластичного контактного взаимодействия, а также расчёт интенсивности изнашивания пар трения в зависимости от нагрузки, микрогеометрии контакта, скорости ...
Added: December 14, 2012
Vasin V. A., Ivashov E., Кузнецов П. С. et al., Электромагнитные волны и электронные системы 2011 № 4 С. 49–55
Рассмотрены особенности проектирования элементов и устройств вакуумного оборудования, предназначенных для реализации экологически чистых и энергосберегающих технологий в электронном производстве. Выполнены расчёты коэффициентов трения материалов, работающих в вакууме, в зависимости от разрежения окружающей среды, для различных случаев контактного взаимодействия, а так же – интенсивности изнашивания пар трения в зависимости от нагрузки, микрогеометрии контакта, скорости скольжения, остаточного ...
Added: April 12, 2012